With a material thickness of 3.0 mm, the bending accuracy can reach within ± 0.1 mm;
The surface is sandblasted and then sprayed.Due to the long-term outdoor use of the product,there is a high requirement for the adhesion of the sprayed coating.
Processing steps:
1、use CNC cutting to obtain shape,size
and performance
2、bending
3、surface sand blasting
4、surface spraying